Beschrijving
Legering | Standaard strengconstructie, mm | Weerstand,Ω/m | Strengdiameter nominaal, mm | Meter per kilo |
NiCr 80/20 | 19×0,544 | 0,233-0,269 | 26 | |
NiCr 80/20 | 19×0,61 | 0,205-0,250 | ||
NiCr 80/20 | 19×0,523 | 0,276-0,306 | 2.67 | 30 |
NiCr 80/20 | 19×0,574 | 2,87 | 25 | |
NiCr 80/20 | 37×0,385 | 0,248-0,302 | 2,76 | 26 |
NiCr 60/15 | 19×0,508 | 0,286-0,318 | ||
NiCr 60/15 | 19×0,523 | 0,276-0,304 | 30 | |
Ni | 19×0,574 | 0,020-0,027 | 2,87 | 21 |
Details
Eigenschappen/graad | Cr20Ni80 | Cr30Ni70 | Cr15Ni60 | Cr20Ni35 | Cr20Ni30 | |
Belangrijkste chemische samenstelling | Ni | Rest | Rest | 55,0-61,0 | 34,0-37,0 | 30,0-34,0 |
Cr | 20.0-23.0 | 28.0-31.0 | 15.0-18.0 | 18.0-21.0 | 18.0-21.0 | |
Fe | ≤ 1,0 | ≤ 1,0 | Rest | Rest | Rest | |
Max. continue servicetemp. van element | 1200 | 1250 | 1150 | 1100 | 1100 | |
Weerstand bij 20oC (μ Ω · m) | 1.09 | 1.18 | 1.12 | 1.04 | 1.04 | |
Dichtheid (g/cm3) | 8.4 | 8.1 | 8.2 | 7.9 | 7.9 | |
Thermische geleidbaarheid (KJ/m · h · oC) | 60,3 | 45,2 | 45,2 | 43,8 | 43,8 | |
Uitbreidingscoëfficiënt van lijnen (α × 10-6/oC) | 18 | 17 | 17 | 19 | 19 | |
Smeltpunt (ca. )( oC) | 1400 | 1380 | 1390 | 1390 | 1390 | |
Rek bij breuk (%) | > 20 | > 20 | > 20 | > 20 | > 20 | |
Micrografische structuur | austeniet | austeniet | austeniet | austeniet | austeniet | |
Magnetische eigenschappen | niet-magnetisch | niet-magnetisch | niet-magnetisch | niet-magnetisch | niet-magnetisch |
Chemische samenstelling | Nikkel, Chroom |
Voorwaarde | Heldere/zure witte/geoxideerde kleur |
Cijfer | Ni80Cr20, Ni70/30, Ni60Cr15, Ni60Cr23, Ni35Cr20Fe, Ni30Cr20 Ni80, Ni70, Ni60, Ni40, |
Voordeel | De metallurgische structuur van Nichrome zorgt ervoor dat ze in koude toestand een zeer goede plasticiteit hebben. |
Kenmerken | Stabiele prestaties; Anti-oxidatie; Corrosiebestendigheid; Stabiliteit bij hoge temperaturen; Uitstekend spoelvormend vermogen; Uniforme en mooie oppervlakteconditie zonder vlekken. |