Beschrijving
Legering | Standaard strengconstructie, mm | Weerstand, ω/m | Strengdiameter nominaal, mm | Meter per kilo |
NICR 80/20 | 19 × 0.544 | 0.233-0.269 | 26 | |
NICR 80/20 | 19 × 0,61 | 0,205-0,250 | ||
NICR 80/20 | 19 × 0.523 | 0.276-0.306 | 2.67 | 30 |
NICR 80/20 | 19 × 0.574 | 2.87 | 25 | |
NICR 80/20 | 37 × 0.385 | 0.248-0.302 | 2.76 | 26 |
NICR 60/15 | 19 × 0.508 | 0.286-0.318 | ||
NICR 60/15 | 19 × 0.523 | 0.276-0.304 | 30 | |
Ni | 19 × 0.574 | 0,020-0,027 | 2.87 | 21 |
Details
Eigenschappen/graad | CR20NI80 | CR30NI70 | CR15NI60 | CR20NI35 | CR20NI30 | |
Belangrijkste chemische samenstelling | Ni | Rest | Rest | 55.0-61.0 | 34.0-37.0 | 30.0-34.0 |
Cr | 20.0-23.0 | 28.0-31.0 | 15.0-18.0 | 18.0-21.0 | 18.0-21.0 | |
Fe | ≤ 1.0 | ≤ 1.0 | Rest | Rest | Rest | |
Max. continue servicetemp. element | 1200 | 1250 | 1150 | 1100 | 1100 | |
Weerstand bij 20oC (μ ω · m) | 1.09 | 1.18 | 1.12 | 1.04 | 1.04 | |
Dichtheid (g/cm3) | 8.4 | 8.1 | 8.2 | 7.9 | 7.9 | |
Thermische geleidbaarheid (kj/m · h · oc) | 60.3 | 45.2 | 45.2 | 43.8 | 43.8 | |
Lijnencoëfficiënt expansie (α × 10-6/oc) | 18 | 17 | 17 | 19 | 19 | |
Smeltpunt (ca.) (OC) | 1400 | 1380 | 1390 | 1390 | 1390 | |
Rek bij breuk (%) | > 20 | > 20 | > 20 | > 20 | > 20 | |
Micrografische structuur | Austenite | Austenite | Austenite | Austenite | Austenite | |
Magnetische eigenschappen | niet -magnetisch | niet -magnetisch | niet -magnetisch | niet -magnetisch | niet -magnetisch |
Chemische samenstelling | Nikkel, chroom |
Voorwaarde | Helder/zuur wit/geoxideerde kleur |
Cijfer | NI80CR20, NI70/30, NI60CR15, NI60CR23, NI35CR20FE, NI30CR20 NI80, NI70, NI60, NI40, |
Voordeel | De metallurgische structuur van Nichrome verleent hen een zeer goede plasticiteit als ze koud zijn. |
Kenmerken | Stabiele prestaties; Anti-oxidatie; Corrosieweerstand; Hoge temperatuur stabiliteit; Uitstekende spoelvormend vermogen; Uniforme en mooie oppervlakte -conditie zonder vlekken. |